NASF/AESF Foundation Research Project #122: Electrochemical Approaches to Treatment of PFAS in Plating Wastewater - 2nd Quarterly Report
The NASF-AESF Foundation Research Board has selected a project on addressing the problem of PFAS and related chemicals in plating wastewater streams, studying PFAS destruction via electrooxidation and electrocoagulation. This second quarter report covers work on electrocoagulation and how it generates amorphous metal hydroxide flocs that can effectively adsorb PFASs in plating wastewater.
#pollution control #nasf
by
Qingguo (Jack) Huang*
College of Agricultural and Environmental Science
University of Georgia - Griffin Campus
Griffin, Georgia, USA
Editor’s Note: For 2021, NASF-AESF Foundation Research Board has selected a project on addressing the problem of PFAS and related chemicals in plating wastewater streams. This report covers the second quarter of work (April-June 2021). A printable PDF version of this report is available by clicking HERE.
Featured Content
Introduction
This project started in January 2021 with the goal of developing applicable electrochemical approaches to remove per- and polyfluoroalkyl substances (PFASs) present in plating wastewaters, including electrooxidation (EO) and electrocoagulation (EC). This project includes three research tasks that are designed to investigate EC, EO and EC-EO treatment train, respectively, designed to probe three hypotheses specified follows:
- EC generates amorphous metal hydroxide flocs that can effectively adsorb PFASs in plating wastewater, which, through an appropriate treatment, can release PFASs into a concentrated solution.
- EO enabled by a Magnéli phase Ti4O7 anode can be used to effectively destruct PFASs in plating wastewater.
- The electrochemical treatment train comprised of EC and EO by Ti4O7 anode can remove and degrade PFASs in plating wastewater more efficiently than either process operated individually.
This report describes part of our continuing effort in Task 1, by evaluating the isotherm-like sorption behavior of the PFASs on EC-generated zinc hydroxide flocs.
The electrocoagulation (EC) process has shown the potential to remove PFASs from water by some recent studies.1,2,3. EC involves the dissolution of charged cations (e.g., Zn2+, Al3+, Fe3+) formed at the sacrificial anode with simultaneous formation of monomeric and polymeric hydroxyl complex species, which can strongly sorb certain pollutants and remove them from contaminated water.4 Lin, et al.1 evaluated PFAS removal using various sacrificial anodes, including aluminum, iron, zinc and magnesium, and found that PFASs can be quickly adsorbed on zinc hydroxide flocs, generated in situ during EC with zinc anode, mainly via hydrophobic interaction. Here in this report, we systematically examined the adsorption behavior of PFAS on the flocs generated during EC with a sacrificial zinc anode.
Experimental
The setup of the EC reactor and the procedure of EC experiments have been described in detail in our first report of this project. In order to further evaluate the adsorption behavior of PFASs on the flocs generated from the zinc anode during EC, a series of EC experiments were conducted using PFAS solution comprised of ten PFASs, including (1) perfluorononanoic acid (PFNA), (2) perfluorooctanoic acid (PFOA), (3) perfluoroheptanoic acid (PFHpA), (4) perfluorohexanoic acid (PFHxA), (5) perfluorooctanesulfonic acid (PFOS), (6) perfluorohexanesulfonic acid (PFHxS), (7) perfluorobutanesulfonic acid (PFBS), (8) fluorotelomer sulfonic acid 8:2 (8:2 FtS), (9) fluorotelomer sulfonic acid 6:2 (6:2 FtS) and (10) fluorotelomer sulfonic acid 4:2 (4:2 FtS). The Initial concentrations were at different levels ranging from 0.001 to 0.1 μm (i.e., 0.001, 0.002, 0.005, 0.01, 0.02, 0.05 and 0.1 μm), and the reaction time was 120 min using a low current density of 0.3 mA/cm2 to prevent foaming. The supernatant was collected from each test cell and analyzed for the ten PFASs. Floc was collected and weighed after freeze drying once reactions were terminated. The data were used to evaluate the sorption capacity of each PFASs constituents and the sorbate-sorbent interactions. The PFASs sorption data were best fitted using the Langmuir isotherm model, Equation 1.
(1)
where Qe is the amount (μmol/g) of PFASs adsorbed at equilibrium; Ce is the equilibrium PFASs concentration (μM) in the solution; Qm represents the adsorption capacity; and kL is the adsorption affinity constant.
Results and discussion
The sorption data of each PFAS obtained by data fitting are shown in Fig. 1(A,B,C) and Table 1. As seen, the adsorption capacity of the ten PFASs followed the order PFOS > PFNA > 8:2 FtS > PFOA > PFHxS > 6:2 FtS > Fluorotelomer sulfonic acid 4:2 (4:2 FtS) > Perfluoroheptanoic acid (PFHpA) > Perfluorohexanoic acid (PFHxA) > PFBS. It is in line with the order of the carbon chain length for each category, while, for a similar carbon chain length, is perfluoroalkanesulfonic acids (PFSAs, including PFOS, PFHxS, and PFBS) > fluorotelomer sulfonic acids (FTSAs, including 8:2 FtS, 6:2 FtS, and 4:2 FtS) > perfluoroalkyl carboxylic acids (PFCAs, including PFNA, PFOA, PFHpA and PFHxA). PFASs with longer carbon chain length tend to be more hydrophobic. This result confirmed that hydrophobic interaction plays a key role in the sorption capacity of PFASs on the zinc hydroxide flocs (Lin, et al. 2015), while charge interactions may also have an impact, as sulfonate head groups tend to have higher charge density than carboxylates in PFASs. According to the adsorption affinity constant (kL) shown in Table 1 (a smaller value indicates greater sorption affinity), the sorption affinity of the ten PFASs followed the order PFHxS > PFOS > PFNA > PFOA > 6:2 FtS > PFHpA > 8:2 FtS > 4:2 FtS > PFHxA > PFBS. The order differs somewhat from that for the sorption capacity, with the larger molecules (PFNA, 8:2 FtS) shifted down in the order. It seems that the larger molecules may be disadvantaged in terms of sorption affinity, while charge interactions play an important role in the intensity of the sorption interactions.
In order to identify if competitive sorption occurred in the ten PFASs solution, EC experiments were also performed to study the Langmuir sorption isotherms of three individual PFASs, including 4:2 FtS, PFOA, and PFOS, on the flocs using the same reaction conditions above. These three PFASs were chosen to represent PFSAs, FTSAs, and PFCAs, respectively. As shown in Fig. 1(D) and Table 1, the sorption capacity of PFOS and PFOA obtained in the individual solutions were much greater than those obtained in the mixture solutions, apparently indicative of competitive sorption effects in the solutions containing multiple PFASs. The sorption capacity of 4:2 FtS was, however, similar for the individual and mixture solutions. This is likely because 4:2 FtS has weaker affinity on flocs, for which competitive sorption effect may not be evident.
Figure 1 - (A, B, C) Langmuir sorption isotherm of the ten PFASs on the flocs (C0 = 0.001 - 0.1 μM, current density = 0.3 mA/cm2, 20 mM Na2SO4, EC time = 120 min); (D) Langmuir sorption isotherm of single 4:2 FtS, PFOA and PFOS on the flocs, respectively. (C0 = 0.002 - 5 μM, current density = 0.3 mA/cm2, 20 mM Na2SO4, EC time = 120 min).
Table 1 - Parameters obtained by fitting isotherm-like sorption data using Langmuir equation.
References
1. H. Lin, et al., “Efficient sorption and removal of perfluoroalkyl acids (PFAAs) from aqueous solution by metal hydroxides generated in situ by electrocoagulation,” Environ. Sci. Technol., 49 (17), 10562-10569 (2015).
2. Y. Wang, et al., “Electrocoagulation mechanism of perfluorooctanoate (PFOA) on a zinc anode: Influence of cathodes and anions,” Sci. Total Environ., 557-558, 542-550 (2016).
3. B. Yang, et al., “Efficient removal of perfluoroalkyl acids (PFAAs) from aqueous solution by electrocoagulation using iron electrode,” Chem. Eng. J., 303, 384-390 (2016).
4. M.Y.A. Mollah, et al., “Fundamentals, present and future perspectives of electrocoagulation,” J. Hazard. Mater., 114 (1-3), 199-210 (2004).
Past project reports
1. Introduction to Project R-122: Summary: NASF Report in Products Finishing; NASF Surface Technology White Papers, 85 (6), 13 (March 2021); Full paper: http://short.pfonline.com/NASF21Mar1.
2. Quarter 1 (January-March 2021): Summary: NASF Report in Products Finishing; NASF Surface Technology White Papers, 85 (12), 13 (September 2021); Full paper: http://short.pfonline.com/NASF21Sep1.
About the author
Dr. Qingguo (Jack) Huang
Qingguo (Jack) Huang is Professor in the Department of Crop and Soil Sciences, University of Georgia, Griffin Campus. He holds a B.S. in Environmental Science (1990) and a Ph.D. in Chemistry (1995) from Nanjing University, China as well as a Ph.D. in Environmental Engineering from the University of Michigan, Ann Arbor, Michigan. Dr. Huang’s research interest focuses on catalysis involved in the environmental transformation of organic pollutants, and development of catalysis-based technology for pollution control and environmental remediation and management. His laboratory has been actively involved in several cutting-edge research topics:
- Enzyme-based technology for water/wastewater treatment and soil remediation
- Electrochemical and reactive electrochemical membrane processes in wastewater treatment
- Catalysis in biofuel production and agro-ecosystem management
- Environmental fate and destructive treatment methods of PFASs
- Environmental application and implication of nanomaterials
He has published over 150 peer-reviewed journal articles, five book chapters and four patents and three patents pending. He has taught three courses at the University Georgia: Introduction to Water Quality, Environmental Measurement, and Advanced Instrumental Analysis in Environmental Studies.
* Principal Investigator (PI) Contact Information:
Qingguo Huang, Ph.D, Professor, Department of Crop and Soil Sciences, University of Georgia
1109 Experiment St., Griffin, GA 30215, USA.
Phone: (770) 229-3302
Fax: (770) 412-4734
E-mail: qhuang@uga.edu
RELATED CONTENT
-
Cyanide Destruction: A New Look at an Age-Old Problem
Cyanide in mining and industrial wastewaters has been around from the beginning, including electroplating processes. This presentation reviews a number of current processes, and in particular, offers new technologies for improvement in cyanide destruction by the most common process, using sodium hypochlorite.
-
Plating Q&A: Can you color stainless steel?
Our expert, Art Kushner, says yes, you can color stainless steel, but it is not a process that is typically performed in a plating shop. Read more about his answer.
-
Is Your Electroplating Waste Hazardous?
Some that bears precious metals is, and there are a host of regulations to consider when recycling.