NASF/AESF Foundation Research Project #122: Electrochemical Approaches to Treatment of PFAS in Plating Wastewater - 4th Quarterly Report
The NASF-AESF Foundation Research Board has selected a project on addressing the problem of PFAS and related chemicals in plating wastewater streams, studying PFAS destruction via electrooxidation and electrocoagulation. This fourth quarter report continues the work on electrocoagulation and electro-oxidation, measuring energy consumption and evaluating methods to remove residual zinc ions from the floc after processing.
#pollution control #nasf
by
Qingguo (Jack) Huang* and Yuqing Ji
College of Agricultural and Environmental Science
University of Georgia
Griffin, GA, USA
Editor’s Note: For 2021, NASF-AESF Foundation Research Board has selected a project on addressing the problem of PFAS and related chemicals in plating wastewater streams. This report covers the fourth quarter of work (October- December 2021). A printable PDF version of this report is available by clicking HERE.
Featured Content
Introduction
This project started in January 2021 with the goal of developing applicable electrochemical approaches to remove per- and polyfluoroalkyl substances (PFASs) present in plating wastewaters, including electrooxidation (EO) and electrocoagulation (EC). This project includes three research tasks that are designed to investigate EC, EO and EC-EO treatment train, respectively, designed to probe three hypotheses specified follows:
1) EC generates amorphous metal hydroxide flocs that can effectively adsorb PFASs in plating wastewater, which, through an appropriate treatment, can release PFASs into a concentrated solution.
2) EO enabled by a Magnéli phase Ti4O7 anode can be used to effectively destruct PFASs in plating wastewater.
3) The electrochemical treatment train comprised of EC and EO by Ti4O7 anode can remove and degrade PFASs in plating wastewater more efficiently than either process operated individually.
The results reported in the previous reports of this project demonstrated the feasibility of a novel treatment train that combines electrocoagulation (EC) with electrooxidation (EO) treatment to remove and degrade per- and polyfluoroalkyl substances (PFASs) from plating wastewater. Electrocoagulation with a zinc anode can effectively remove PFASs from water, particularly the long-chain PFASs (C7 - C10) that are present in plating wastewater, by concentrating them on the flocs or in the foams generated during EC. Both the flocs and the foams can be dissolved by acid to recover and concentrate the PFASs in controlled volumes. The concentrated PFASs in the acid solutions were efficiently destroyed using EO treatment with a Ti4O7 anode at 10 mA/cm2, and no supplemental electrolyte was needed for the flocs dissolved in solution. This electrochemical-based EC-EO treatment train can likely economically separate, concentrate and destroy PFASs in plating wastewater.
This report describes our continuing effort in Task 3. First, we calculated the energy consumption of the EO treatment process in terms of EE/O that is defined as the electrical energy required to reduce the concentration of a pollutant by one order of magnitude (kWh/m3).1 Second, we evaluated means to remove residual zinc ions that may exist after the EO treatment of the acid dissolved solution of zinc flocs.
Experimental
Calculation of EE/O was based on the results of the experiment of EO treatment reported earlier, which is presented in Fig. 2 in the 3rd report.2 In that experiment, three different concentrated solutions prepared through the electrocoagulation (EC) process were subjected to electrooxidation (EO) treatment using Magnéli phase Ti4O7 anodes at the current density of 10 mA/cm2. Solution I was the acid dissolved solution of PFASs-laden floc generated using a low current density condition after 120 min (0.3 mA/cm2, 0.005 μM each of 10 PFASs). Solution II was the acid dissolved PFASs-laden floc solution obtained through EC treatment under the high current density condition after 60 min (5 mA/cm2, 0.5 μM each of 10 PFASs). The foam collected during this EC process was supplemented with 20 mM Na2SO4 to a final volume of 10 mL as Solution III.
An experiment was performed to assess the methods of removing zinc ions from the solution produced by acid dissolution of the zinc hydroxide flocs generated during the EC process. Specifically, removal of zinc ions was achieved by precipitation with the addition of Na2S or Na2CO3. In this experiment, EC was first conducted in a 20-mM Na2SO4 solution with PFASs at 0.3 mA/cm2 for 120 min or at 5 mA/cm2 for 60 min. The entire solution, including flocs, was then collected and filtered through a 0.22-μm acetate membrane filter. The EC flocs from both current density conditions were then collected and dissolved in 10 mL 4.0M H2SO4, respectively. Na2S or Na2CO3 was then added to the solution at different dosages. The concentration of Zn2+ in the solution was determined using an ICP-MS (Perkin Elmer Elan 9000 inductively coupled plasma equipped with a mass spectrometer),3 with a detection limit of 0.05 mg/L.
Results and discussion
The EE/O (kWh/m3) of PFAS degradation in the three solutions described above was calculated by equation 1,1
(1)
where Ucell is the average cell voltage during EO treatment (V), I is the applied current (A), V is the volume of the reaction solution (L). t90% is the time (hr) for 90% PFAS removal that was calculated by equation 2:
(2)
where C/C0 is 10% and k (min-1) is the pseudo-first-order rate constant for the degradation of different PFASs in the three solutions that was obtained by fitting the data of PFAS degradation, presented in Fig. 1 of the 3rd report,2 to the pseudo-first-order rate model, which are listed in Table 1.
The calculated EE/O values of PFASs degradation in concentrated solution are shown in Table 2. The EE/O varies from 0.34 to 15.7 kWh/m3 for different PFASs in different solutions. It appears that the EE/O was lower for the long-chain PFAS, e.g., PFNA, PFOA, PFOS, than the shorter ones, e.g., PFBS and PFHxA. It is notable that the EE/O for the PFASs frequently present in plating wastewater is particularly low, for example, it was 0.66 (kWh/m3) for 6:2 FTS, 0.55 (kWh/m3) for PFOS, and 0.95 (kWh/m3) for PFOA in solution I. Such EE/O levels are considered favorable for applications in wastewater treatment.
The result of the experiment to assess the methods of removing zinc ions from the solution by precipitation with the addition of Na2S or Na2CO3 is shown in Figure 1. It is apparent that the zinc concentration remaining in the solution decreased dramatically as the added Na2S or Na2CO3 increased, because of the precipitation of ZnS or ZnCO3. Nearly all dissolved Zn2+ was precipitated out when sufficient salts had been added. This proves that chemical precipitation can be used as an effective means to remove the residual zinc in the final effluent of the proposed EC-EO treatment train.
Table 1 - The pseudo-first-order rate constant (min-1) of PFASs in concentrated solution in EO process.
Table 2 - EE/O (kWh/m3) for PFASs degradation in concentrated solution during EO process.
Figure 1 - Concentration of zinc ions in the solution at different current densities and with Na2S or Na2CO3 added at different dosages.
References
1. K. Yang, H. Lin, S. Liang, R. Xie, S. Lv, J. Niu, J. Chen and Y. Hu, “A reactive electrochemical filter system with an excellent penetration flux porous Ti/SnO2–Sb filter for efficient contaminant removal from water,” RSC Adv., 8 (25), 13933-13944 (2018).
2. Q. Huang, “NASF/AESF Foundation Research Project #122: Electrochemical Approaches to Treatment of PFAS in Plating Wastewater - 3rd Quarterly Report,” NASF Surface Technology White Papers, 86 (6), 11-14 (2022); http://short.pfonline.com/NASF21Dec2.
3. Y. Shu, N. Zheng, A. Zheng, T. Guo, Y. Yu and J. Wang, “Intracellular zinc quantification by fluorescence imaging with a FRET System, Anal. Chem., 91 (6), 4157-4163 (2019).
Past project reports
1. Introduction to Project R-122: Summary: NASF Report in Products Finishing; NASF Surface Technology White Papers, 85 (6), 13 (March 2021); Full paper: http://short.pfonline.com/NASF21Mar1.
2. Quarter 1 (January-March 2021): Summary: NASF Report in Products Finishing; NASF Surface Technology White Papers, 85 (12), 13 (September 2021); Full paper: http://short.pfonline.com/NASF21Sep1.
3. Quarter 2 (April-June 2021): Summary: NASF Report in Products Finishing; NASF Surface Technology White Papers, 86 (3), 18 (December 2021); Full paper: http://short.pfonline.com/NASF21Dec2.
4. Quarter 3 (July-September 2021): Summary: NASF Report in Products Finishing; NASF Surface Technology White Papers, 86 (6), 16 (March 2022); Full paper: http://short.pfonline.com/NASF22Mar2.
About the author
Qingguo (Jack) Huang is Professor in the Department of Crop and Soil Sciences, University of Georgia, Griffin Campus. He holds a B.S. in Environmental Science (1990) and a Ph.D. in Chemistry (1995) from Nanjing University, China as well as a Ph.D. in Environmental Engineering from the University of Michigan, Ann Arbor, Michigan. Dr. Huang’s research interest focuses on catalysis involved in the environmental transformation of organic pollutants, and development of catalysis-based technology for pollution control and environmental remediation and management. His laboratory has been actively involved in several cutting-edge research topics:
Enzyme-based technology for water/wastewater treatment and soil remediation
Electrochemical and reactive electrochemical membrane processes in wastewater treatment
Catalysis in biofuel production and agro-ecosystem management
Environmental fate and destructive treatment methods of PFASs
Environmental application and implication of nanomaterials
He has published over 160 peer-reviewed journal articles, five book chapters and four patents and three patents pending. He has taught three courses at the University Georgia: Introduction to Water Quality, Environmental Measurement, and Advanced Instrumental Analysis in Environmental Studies.
* Principal Investigator (PI) Contact Information:
Qingguo Huang, Ph.D, Professor, Department of Crop and Soil Sciences
University of Georgia
1109 Experiment St.
Griffin, GA 30215, USA.
Phone: (770) 229-3302 Fax: (770) 412-4734
E-mail: qhuang@uga.edu
RELATED CONTENT
-
Smut and Desmutting
Question: I am new to this industry and have heard about smut and desmutting operations.
-
Nitric Acid Passivation and EH&S Impact
I am looking for safety/environmental requirements to set up a nitric acid cleaning and passivation system.
-
Corrosion Testing of Automotive Coatings
Exposure to road salts, UV radiation, heat, moisture and chipping from kicked-up road debris can quickly degrade an automotive coating system.