HUI uses powder coating on its custom medical carts.

Many of the custom medical carts that HUI manufactures have a powder coated finish, and as with any finish applied to any product, the powder coating we apply needs to be tested to ensure that the finish is going to last.

The following is a description of some of the tests our company commonly uses to validate that the powder coated finishes are in tolerance, properly cured and ready to stand up to the environmental conditions your carts will be used in.

Adhesion Tests

The scratch test is performed by cutting a crosshatched grid pattern into the coating all the way down to the substrate.

Crosshatch. The crosshatch test is designed to test the adhesion of the powder coating to the metal substrate. It’s performed by cutting a crosshatched grid pattern into the coating all the way down to the substrate. A special pressure-sensitive tape is then applied to the crosshatched area and then removed quickly at close to a 180-degree angle. The area is then inspected to see if any of the coating is lifted away from the substrate.

Mandrel Bend

Mandrel Bend. This test checks the elasticity and the adhesion of the powder coating to the substrate. A cured sample panel is placed into a small device that bends the panel over onto itself. The coating should not crack or lose adhesion in the area of the bend.

The sample panel is placed into the testing machine where a ball is dropped onto it to produce a deep depression.

Impact Test. Similar to the mandrel bend test, the impact test deforms a sample panel in order to test the adhesion of the powder coating. The sample panel is placed into the testing machine where a ball is dropped onto it to produce a deep depression. Here again, the powder coated finish should not crack or lose adhesion to the substrate in the impacted area.

Durability Test

Salt Spray Test. This is a corrosion resistance test and is performed by scribing a line or “X” onto the surface of a finished powder coated panel. The panel is then placed into a chamber where a corrosive mist is applied. The panel is taken out of the chamber at set time intervals and the distance that the coating has “crept” away from the scribed line is measured and recorded. If the amount of creep does not exceed the allowable distance in the predetermined time intervals, the panel passes the test.

Cure and Finish Tests

MEK Rub Test. This test is used to ensure proper cure of the powder coating to the substrate. Methyl ethyl ketone (MEK) is applied to a surface of the part or panel and then rubbed with a cotton swab. The area is observed for degradation or loss of paint adhesion to the substrate.

Color Match. Once our powder coated parts have cured and cooled off after being in the bake oven, the finished color is compared to an approved color chip sample. This visual inspection is the most common and quickest method to check the color. If there is a variance, the color can then be measured using a photo spectrometer to provide data that can be compared to a known sample and tolerance range for the specific color.

Gloss Test – The gloss of a finished powder coated part is validated by measuring the specular reflection of its surface.

Gloss Measurement. The gloss of a finished powder coated part is validated by measuring the specular reflection of its surface. This test is performed using a gloss meter, which shines a light onto the surface of the part at a fixed angle, then measures the amount of light reflected off it. If the measurement is out of tolerance, it may be an indication that the powder coating has not cured properly.

Coating Thickness Test

To achieve the best coating performance, each powder has a specified thickness range it must be applied within. HUI takes this measurement at two different stages during the powder coating process. Our powder room technician uses a dry mil gage to take the first measurement right after the part comes out of the powder booth. The technician can then relay to the painters whether they’re applying the correct amount of powder onto the parts. 

This immediate feedback is beneficial because it catches possible lightly or heavily coated parts before the powder is cured and it’s too late to fix the problem. After the parts have cured, the mil thickness is checked again to verify the coating thickness is within tolerance for the specified powder.

At HUI, we validate our painting processes to ensure that a medical cart’s finish stays beautiful and durable, so that customers receive the finish they desire.  

Greg Binversie is an engineer with HUI Manufacturing. For information, visit medicalcarts.org.


Originally published in the April 2017 issue.

Powder Coating Institute
Custom Making Solutions
UV Powder Coating  for Heat Sensitive Substrates
Steelman Industries Inc.
complete finishing application systems
Your Best Finish Starts With Us!
Mocap Masking Caps Plugs Tapes
The Finishing Industry’s Education and Networking Resource
Bulk Chemicals, Inc.
New Acid-Free Bright Nickel Process
Parts Cleaning Conference
Fischer Technology, Inc.

Related Content

Electroplating

A Chromium Plating Overview

An overview of decorative and hard chromium electroplating processes.

Read More
Electroplating

Choosing and Troubleshooting Copper Electroplating Processes

Learn more on this inexpensive and highly efficient process.

Read More
basics

Calculating the Cost of Powder Coating

How can you calculate the cost of powder coating a component if you only know its surface area? Powder coating expert Rodger Talbert has the answer.

Read More
basics

Coating Systems with the Best Long-Term Performance

The best protection against corrosion and UV exposure, says Axalta’s Mike Withers, is electrocoat and a super durable powder coating.

Read More

Read Next

automotive

The 2024 Ford Mustang: All the Colors Available

Although Chevrolet has announced the end of the Camaro and Dodge is offering “Last Call” editions of the Charger and Challenger, the Ford Mustang is launching to its seventh generation.

Read More
Powder Coating

Powder Coating 4.0: Smarter, Faster, More Efficient and Connected

New tools reduce cost and waste, lower manufacturing footprint of powder coating operations.

Read More
Pollution Control

Episode 42: An Interview with Robin Deal, Hubbard-Hall

Hubbard-Hall wastewater treatment specialist Robin Deal discusses the latest trends in wastewater management. 

Read More
UV Cured Powder for Heat Sensitive Substrates