Deflectometry is used to detect paint defects

Deflectometry is used to detect any defects on the painted surfaces of the BMW 1 Series, X1 and X2 models produced at the company’s plant in Regensburg, Germany.
Photo Credit: All photos courtesy of BMW

Everyone is talking about AI. BMW is doing something about it — or more specifically, with it, as it is deploying AI to achieve superb surfaces on the 1 Series, X1 and X2 models that it is producing at Plant Regensburg in Germany.

As is common in automotive paint shops, after the topcoat is applied, surface inspection is conducted. Here they are using deflectometry to assess the surface. Black and white striped patterns are projected on the vehicle and then cameras are used to scan and detect any flaws on the reflective paintwork. Simply: if there is a defect, it affects the striped pattern.

While using deflectometry is typical in automotive paint facilities, what’s not always the case is that the BMW system cameras register the locations of the defects and the data is uploaded to a computer system. Then a digital 3D image of the deviation is created, classified and stored. Each scanned body — and they are producing up to 1,000 vehicles per day in the factory — has its own profile created; that is then used for the subsequent surface processing. The data is stored in the cloud.

Ordinarily, this scanning involves highly trained human operators. BMW’s Daniel Poggensee, a structural planner for Surface Technology, says, “The system already knows as much today as our best employees combined. We used the knowledge of our entire team to finalize the system; the functioning of the equipment relies on our associates’ unique expertise. We channeled their experience into the programming — on this basis, the algorithm now recognizes and objectively decides which features need post-processing.”

What’s more, the system determines the optimal order in which the surface flaws are addressed by an AI-based, automated surface processing system.

So there is a given body. The scanned and processed data is delivered to a processing booth where there are four robots. Here the problem areas are being sanded, having polishing compound applied, and being polished. Attachments and sandpaper are automatically swapped out.

Robots remove paint defects in an automotive facility

Vehicles move into a booth where robots remove the defects from the surface. The locations of the defects and the order in which they are addressed are based on an AI assessment.

Work Where It Is Needed

Here’s the notable aspect of the operation, which BMW says is the first end-to-end digitized and automated process for inspecting, processing and marking painted vehicle surfaces in serial production:

Stefan Auflitsch, head of Production Paint Application and Finish at BMW Group Plant Regensburg, explains, “What is unique here is that the robots work on each body exactly where needed — because the tiny specks and bumps that can appear after the topcoat is applied and that we want to remove are in different spots on each vehicle.

“Robots are normally programmed to follow the same pattern until they are reprogrammed. Using artificial intelligence allows them to work in a more tailored manner. With up to 1,000 vehicles going through the finishing process every working day, that adds up to 1,000 unique processes.”

Consider: Whereas conventionally controlled robots are highly deterministic in terms of following a set pattern — A to B to C to D to E — the AI-controlled robots are going to the places on the painted body where the defects need to be addressed and in the most efficient order — B to D to A to E, possibly not needing to go to C for a given vehicle, or to any other location as required (F, G, H, etc.).

Robotic polishing

The robots change their end effectors as needed for sanding and polishing the surfaces.

Still a Human Touch

All of that notwithstanding, people are brought into the process at Plant Regensburg, too.

Turns out that the robots aren’t good at dealing with the edges of the vehicle body nor close up to joints, such as at the doors. Also, the fuel filler cap is too fragile for robot processing.

So BMW associates are used to address problem areas. But even here, advanced tech is used to ensure that all defects are addressed: a laser projector is used to “mark” the issues on the sheet metal so the workers know where to go.

Poggensee thinks the data being accumulated in the cloud might allow them to determine whether there are process inconsistencies such that it “will enable us to prevent faults from occurring in the first place.”

And that would be the best-painted surface of all.

Your Best Finish Starts With Us!
ENGINEERED PAINT BOOTHS & FINISHING SOLUTIONS
Precision gear pumps
Carlisle Fluid Technologies Finishing Solutions
Parts Cleaning Conference
Mocap Masking Caps Plugs Tapes
The Finishing Industry’s Education and Networking Resource
Bulk Chemicals, Inc.
Filtration
New Acid-Free Bright Nickel Process
More blasting. Less part handling.
Pretreatment Washer and Finishing Equipment

Related Content

automotive

Henry Ford Is Still Right When It Comes to Color

Who would have imagined that more than 100 years after his famous statement about any color as long as it’s black would still have relevance of a sort?

Read More
Liquid Coating

How to Avoid Mud Cracking

Julie Holmquist of Cortec Corporation discusses ways to avoid mud cracking defects when applying anticorrosion coatings.

Read More
Powder Coating

Conveyors and Paint Systems

Choosing the right conveyor system, coating technology, and ancillary equipment.

Read More
Liquid Coating

Surface Prep Solution for Rusted Rebar in Concrete

Julie Holmquist of Cortec Corporation discusses passivating corrosion on rebar and other reinforcing metals.

Read More

Read Next

automotive

Henry Ford Is Still Right When It Comes to Color

Who would have imagined that more than 100 years after his famous statement about any color as long as it’s black would still have relevance of a sort?

Read More
automotive

The 2024 Ford Mustang: All the Colors Available

Although Chevrolet has announced the end of the Camaro and Dodge is offering “Last Call” editions of the Charger and Challenger, the Ford Mustang is launching to its seventh generation.

Read More
automotive

Pretend Your Audi EV Is the Prototype

While camouflage car coverings are meant to disguise surfaces of development vehicles, what Audi is doing to the RS e-tron will turn a whole lot of heads — and it is an electric vehicle that you can have in your own driveway.

Read More
Precision gear pumps